Pre-Preg Tapes
This method is primarily used to provide a composite substrate for the winding of antenna. Our current process material achieves the following minimum properties:-
- Density 1.23g/cm³ (76lbs/ft³) at 23°C (73.4°F)
- Tg (after postcure) Onset 200°C (392°F)
- Peak Tan δ: 220°C (428°F)
- Low Tool C.T.E. 10.5-12 x 10-6 /°C
- Fibre Volume Fraction 55-60%V/V
This composite substrate will withstand operation temperatures of 185°C and pressures up to 20,000PSI
Capacity Envelope: - Ø12” (300mm) x 393” (10m) long